Laser Induced Defects for Testing and Calibration

Laser Induced Defects for Testing and Calibration: Laser cut defect in cast iron material   Defect is 250um wide x 350um deep.  Potomac has developed a broad array of technologies capable of fabricating Defects and Calibrated Leak Orifices as small as 1 micron.